Poor adhesion Poor adhesion

Poor adhesion

Poor adhesion

Poor adhesion

Ink film is too heavy

Run thinner ink film, Stronger ink, Change the ink to cure deeply

Low surface energy < 38dynes/cm.

Treat the substrate with a water based or solvent based primer or else change tochemically coated stock

Overcuring

Reduce UV power or multiple curing to avoid overcuring

Undercured dark colour

Decrease the press speed and try lowring the ink film weight

Weak bonding of laminated stock.

Check the lamination bonding for weakness