Low rub & scratch resistance Low rub & scratch resistance

Low rub & scratch resistance

Low rub & scratch resistance

Low rub & scratch resistance

The films not pre treated

Insufficient bond. Either apply corona or primer. It is recommended to maintain surface tension in between 40mN/m to 44mN/m

Higher film weight of UV OPV

Control the film weight for better results

The curing is not suffeciently done

Consider checking curing of each colour & OPV

Poor wetting of UV OPV

Please change the UV OPV with new one

For more information, please contact us.