Blocking

Blocking

Excess ink retention to obtain desired strength

Increase the strength of the ink

The ink has high coating weight

Try reducing the film weight, it will reduce the coating weight

High Temperature & humidity

Maintain pressroom temp 20-30 deg C & Relative Humidity 50-60% to keep in control

Low gramage substrate

Reduce stack height to control gramage substrate

Spray powder used

Do not use spray powder for better results

Undercured

Clean UV lamp, Check output of UV lamp, Distance between application & curing must be reduced, Reduce speed

For more information, please contact us.

Connect with DIC