Excessive slip package is present in the first down ink
Reformulate ink for best trapping properties
Ink choice is improper for substrate
Reformulate ink for specific substrate
Ink is brittle due to insufficient plasticizer
Add a small amount of plasticizer
Ink is not drying properly
Add faster solvents, increase air and heat
Re-worked ink with out of balance pigment to vehicle ratio
Remake ink or refresh ink with pigment and resin
Surface is not ink or lacquer receptive
Treat substrate, change ink or u
Web temperature is too low for the substrate and ink
Increase web temperature to adequate level for substrate and ink