Ink choice is improper for a substrate

Reformulate ink for specific substrate.

Ink is brittle due to insufficient amount of plasticizer

Add small amount of plasticizer and check again

Ink is not drying properly

Add faster drying solvents and/or increase air and heat delivery. Thin inks If possible.

Ink viscocity is too high

Reduce ink viscosity to proper level

Re-worked ink has an out of balance pigment to vehicle ratio

Remake ink or refresh ink with pigment and resin

Surface is not ink or lacquer receptive

Treat substrate, change ink or use a printer

Web temperature is too low for substrate and ink

Increase web temperature to adequate level for substrate